- productspecificaties
- Verpakkingen
- vraag offerte
Very good welding and wetting characteristics and high resistance to cracks and fissures. Extreme good deposition rate compare to MMA.High strength and good bonding weld metal..
Not required
Build-up of cast iron and alloyed grey-cast iron Well suited for warm and in special applications for cold welding. Used to fill-in voids and pores, build-up of worn-down parts.
Build-up of cast iron and alloyed grey-cast iron Well suited for warm and in special applications for cold welding. Used to fill-in voids and pores, build-up of worn-down parts.
Very good welding and wetting characteristics and high resistance to cracks and fissures. Extreme good deposition rate compare to MMA.High strength and good bonding weld metal..
DIN GG15 – GG40, GGG40 - GGG70, GTS35 - GTS 65
ASTM: A48 Class 25 B - A48 Class 60 B, A536 Grad 60-80
FGL 150- FGL 400, FGS 400 12 - FGS 600 3, MN350 10 - MN650 3



| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
|---|---|---|---|---|
| As Welded | 200 HB |