- productspecificaties
- Verpakkingen
- vraag offerte
The weld deposit is applicable in a low sulphur, carbon enriching atmosphere up to 1175° C and has an excellent creep strength and a good resistance against carburization and oxidation.
Not required
Joining and cladding high heat resistant NiCr-steels of the same kind and Cast steels in a low sulphourus invironment.
Joining and cladding high heat resistant NiCr-steels of the same kind and Cast steels in a low sulphourus invironment.
The weld deposit is applicable in a low sulphur, carbon enriching atmosphere up to 1175° C and has an excellent creep strength and a good resistance against carburization and oxidation.
1.4898,
GX45NiCrNbSiTi45-35
Parralloy H46M, Centralloy ET45, Lloyds T80, Lloyds T75MA, Manaurite XT/XTM, E3545Nb-MA






| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
|---|---|---|---|---|
| As Welded | 460 | 600 | 10 | HRc |