T92/P92 steel is commonly used at service temperatures up to 620°C. V, Nb and N additions provide this ‘creep strength enhanced ferritic’ (CSEF) alloy with improved high temperature creep resistance compared to standard CrMo creep resistant alloys.
Not required
TIG/GTAW wire for high temperature, creep resistant, modified 9%Cr1%Mo martensitic steel (T92/P92). Alloy T92/P92 is widely used in the power generating industry for fossil fuel ultra-super-critical (USC) power plant boilers and turbines; the alloy is also finding applications in the chemical and oil and gas industries.
TIG/GTAW wire for high temperature, creep resistant, modified 9%Cr1%Mo martensitic steel (T92/P92). Alloy T92/P92 is widely used in the power generating industry for fossil fuel ultra-super-critical (USC) power plant boilers and turbines; the alloy is also finding applications in the chemical and oil and gas industries.
T92/P92 steel is commonly used at service temperatures up to 620°C. V, Nb and N additions provide this ‘creep strength enhanced ferritic’ (CSEF) alloy with improved high temperature creep resistance compared to standard CrMo creep resistant alloys.
P92: 9%Cr1.7%W0.5%Mo,
1.4901
X10CrWMoVNb 9 2
ASTM A213 Gr. T 92; A355 Gr. P92; A187 F92, A369 FP92; A1017 Gr 92
KA-STBA29; KA-STPA29 NF 616







| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
|---|---|---|---|---|
| 730°C- 760°C 3h | 550 | 630 | 17 | HRc |