BÖHLER FOX alform 700
CEWELD® E 11018-M is a Mn, Ni, Cr and Mo alloyed highly basic electrode for welding low-alloy steels with a tensile strength ≤ 700 MPa. Used in offshore, crane construction, heavy transport machinery, lifting equipment, etc.
CEWELD® E 11018-M is a Mn, Ni, Cr and Mo alloyed highly basic electrode for welding low-alloy steels with a tensile strength ≤ 700 MPa. Used in offshore, crane construction, heavy transport machinery, lifting equipment, etc.
CEWELD® E 11018-M is crack resistant and well suited for low temperatures. It shows very good ductility down to -60 °C.
The preheating, interpass temperature and post-weld treatment should be selected as for the base metal.
The hydrogen content is HD < 3 ml/100 g in the weld metal.
1.8914, 1.8927, 1.8931, 1.8928, 1.7147, 1.7149, 1.8734
S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1
L480 - L550, X65, X80, X90, X100, HY 80, HY 100
ASTM A 514 Gr. F, H, Q; A 709 Gr. 100 Type B, E, F, H, Q; A 709 Gr. HPS 100W
Weldox 700, Dillimax 690, Hardox, Naxtra 63, Naxtra 70, Optim 700 mc plus, Weldox 500, Hardox, Domex 460 MC, Domex 500 MC, Domex 550 MC, Domex 600 MC, Domex 650 MC, Domex 700 MC, Hardox 400, XAR 400, Dillidur 400, Oceanfit 100, Oceanfit 690, alform plate 620 M, 700 M, aldur 620 Q, 620 QL, 620 QL1, aldur 700 Q, 700 QL, 700 QL1





| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
|---|---|---|---|---|---|
| -50°C | |||||
| As Welded | 705 | 770 | 20 | 65 | HRc |
CEWELD® E 12018-G is a basic electrode with excellent welding characteristics, recommended for welding fine grained similar alloyed high yield strength steel (< 830 MPa)
Used in the heavy boiler and pressure vessels industry, highly stressed structural components, pipes, etc…
CEWELD® E 12018-G is a basic electrode with excellent welding characteristics, recommended for welding fine grained similar alloyed high yield strength steel (< 830 MPa)
Used in the heavy boiler and pressure vessels industry, highly stressed structural components, pipes, etc…
CEWELD® E 12018-G have good radiographic quality of the joints and very good impact test values at low temperatures. Hydrogen content HD < 4 ml/100g in the weld metal.
Reh < 790 MPa Iso 15608: 3.2 ( > 690(700) MPa )
1.7147, 1.7149, 1.8734, 1.8894, 1.8914, 1.8927, 1.8931, 1.8938, 1.8951, 1.8974
S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1, TStE 770 V, S770QL, 20MnCr65, 28CrMn4-3
L480 - L550, X65, X80, X90, X100
ASTM A 514 Gr. F, H, Q; A 709 Gr. 100 Type B, E, F, H, Q; A 709 Gr. HPS 100W
Weldox 700, Dillimax 690, Hardox, Naxtra 63, Naxtra 70, Optim 700 mc plus, Weldox 500, Hardox, Domex 460 MC, Domex 500 MC, Domex 550 MC, Domex 600 MC, Domex 650 MC, Domex 700 MC, Hardox 400,Strenx 700; XAR 400, Dillidur 400, Oceanfit 100, Oceanfit 690, alform plate 620 M, 700 M, aldur 620 Q, 620 QL, 620 QL1, aldur 700 Q, 700 QL, 700 QL1, Salzgitter S700MC, Ympress Steel E690 TM, S700MC, Amstrong Ultra 650MC, 650 MCt, 700 MC,HR700LA





| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
|---|---|---|---|---|---|
| -50°C | |||||
| As Welded | 840 | 970 | 18 | 50 | HRc |