Type
Submerged Arc wire for welding temperature resistant boiler steels and base metals.

Submerged arc welding wire for high temperature creep resistant 2,45%Cr 1,0%Mo ferritic steel. These steels are used for creep resisting applications up to ~550°C.  The wire has low levels of tramp elements (e.g. Sn, As, Sb and P) providing a low Bruscato Factor (X< 10 ppm) for temper embrittlement resistant applications. Recommended flux: FL 155

Not required

classification
AWS
A 5.23: EB3
EN ISO
24598-A: S CrMo2
Anwendungen

Typical applications in power generation plant include steam piping, turbines and boilers; the alloy also finds applications in the chemical and petrol-chemical industries.

Type
Submerged Arc wire for welding temperature resistant boiler steels and base metals.
Anwendungen

Typical applications in power generation plant include steam piping, turbines and boilers; the alloy also finds applications in the chemical and petrol-chemical industries.

Eigenschaften

Submerged arc welding wire for high temperature creep resistant 2,45%Cr 1,0%Mo ferritic steel. These steels are used for creep resisting applications up to ~550°C.  The wire has low levels of tramp elements (e.g. Sn, As, Sb and P) providing a low Bruscato Factor (X< 10 ppm) for temper embrittlement resistant applications. Recommended flux: FL 155

Klassifikation
AWS
A 5.23: EB3
EN ISO
24598-A: S CrMo2
F-nr
6
FM
3
Geeignet für

2,25% Cr, 1% Mo

 1.7015, 1.7131, 1.7147, 1.7380, 1.7337, 1.7262, 1.7258, 1.7350, 1.7357, 1.7375, 1.7379, 1.7383, 1.7385, 1.7707, 1.8075

10CrMo9.10, 12CrMo9-10, 10CrSiMoV7, 12CrSiMo8, 30CrMoV9, GS-18CrMo9.10, 15CrMoV5-10, 16CrMo4-4, 15CrMo5, 24CrMo5, 22CrMo4-4, GS-17CrMo5-5, 15Cr3, 16MnCr5, 20MnCr5, 10CrSiV7,  

ASTM: A 387 Gr. 22, A217 Grade WC9, A335 Gr. P22, A217 Gr. WC9, A182 F22, A182 T22, A1031 Gr.5015,  A1031 Gr.5115, A1031 Gr.4820

Zulassungen
CE
Schweißpositionen
PA
PB
PC
Rücktrocknung

Not required

Analyse
C Si Mn P S Cr Ni Mo V Cu N Al Nb+Ta Ti Zr Nb
0.1 0.25 0.6 0.01 0.01 2.45 1
Mechanische Gütewerte
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Impact Energy (J) ISO-V Hardness
RT -20°C
690°C±15°C 3h 490 600 24 100 50 HRc