STELLITE 1 ALLOY
Outstanding hardfacing alloy against abrasion and corrosion combined with high temperatures.
Not required
Pump sleeves, expeller screws, impellors, plastic recycling, mixer blades for rubber, valves, seats etc.
Pump sleeves, expeller screws, impellors, plastic recycling, mixer blades for rubber, valves, seats etc.
Outstanding hardfacing alloy against abrasion and corrosion combined with high temperatures.
Stellite 1 alloy for cladding,



| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
|---|---|---|---|---|
| As Welded | 55 HRc |
CEWELD AA DUR 1 deposits a cobalt-base alloy with an austenitic-ledeburitic structure. This is the hardest of the standard cobalt-base alloys. It has a high resistance to corrosion (especially to reducing acids and impact), extreme wear and temperature shocks. The alloy is only machinable by grinding. Best used on wear pads, rotary seal rings, pump sleeves and centerless grinder work rests.
140°C / 24 hr
Pump sleeves, expeller srews, plastic recycling, mixer blades for rubber, valves, seats etc..
Pump sleeves, expeller srews, plastic recycling, mixer blades for rubber, valves, seats etc..
CEWELD AA DUR 1 deposits a cobalt-base alloy with an austenitic-ledeburitic structure. This is the hardest of the standard cobalt-base alloys. It has a high resistance to corrosion (especially to reducing acids and impact), extreme wear and temperature shocks. The alloy is only machinable by grinding. Best used on wear pads, rotary seal rings, pump sleeves and centerless grinder work rests.
ER CoCr-C / Co3
Stellite 1



| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
|---|---|---|---|---|
| As Welded | 53 HRc |